Product introduction: It is third generation of polypropylene nucleating agent. It has better biological fitness compare with 2nd generation product.
Product structure:
Product index:
Item |
Unit |
Quality index |
Appearance |
-- |
White powder |
Content |
% |
≥99.0 |
Melting point |
℃ |
≥240 |
Loss on heating (105℃±3℃) |
% |
≤0.5 |
Ash content |
% |
≤0.2 |
Product uses:
It is sorbitol type organic nucleating agent widely used nucleating modification of polypropylene articles. It can improve transparency, glossiness, rigidity, flexural modulus, tensile strength, distortion temperature and size stability, shorten molding cycle and promote production efficiency of polypropylene film, sheet and injection molding products.
Packaging:
Should be preserved in ventilated, dry and cool place
Be packed with standard paper can lined with PE plastic bag
Net weight: 15kg
|